Figure 1From: Nanoparticulate PdZn as a Novel Catalyst for ZnO Nanowire GrowthRepresentative SEM (left) and TEM (right) images of samples a 2 (stainless steel grid, dip coated, deposition temp. 640°C), b 9 (stainless steel grid, droplet coated, deposition temp. 760°C), c 11 (Ti grid, droplet coated, deposition temp. 680°C), d 12 (Ti grid, droplet coated, deposition temp. 820°C), e Si reference wafer, spin coated. c(cat) = 0.490 mg/ml (see Electronic Supplementary Information)Back to article page