Figure 6From: Field Dependence of the Spin Relaxation Within a Film of Iron Oxide Nanocrystals Formed via Electrophoretic DepositionZFC/FC measurement of m(T) at parallel applied fields of 25, 100, 200, and 500 Oe. Filled symbols represent the ZFC data points, and open symbols represent the FC data pointsBack to article page