Figure 5From: Crystallization of Ti33Cu67 metallic glass under high-current density electrical pulses SEM micrograph of the Ti 33 Cu 67 ribbons electrochemically etched in HNO 3 -CH 3 OH. (a, b) N1; (c, d) N2; (e, f) N3; (g, h) conventionally annealed at 773 K.Back to article page