Figure 2From: Nanopatterning on silicon surface using atomic force microscopy with diamond-like carbon (DLC)-coated Si probe AFM images of the grooves. (a-b) The AFM images of the grooves scratched at 1 μm/s of scratch speed under different applied forces in the forward scratch. (c) The size of the scratched grooves as a function of the applied normal force.Back to article page