Figure 4From: Annealing of gold nanostructures sputtered on polytetrafluoroethylene AFM images of pristine (PTFE) and Au-coated (PTFE/Au) samples (thickness of 20 nm). Before (RT) and after annealing at 300°C. Numbers in frames are measured surface roughnesses R a in nanometers.Back to article page