Figure 3From: The nitridation of ZnO nanowiresTypical RT PL of ZnO NWs grown on 1.0 nm Au/Si(001) at 550°C. The inset shows a plot of α2 versus energy from ZnO NWs grown on 0.5 nm Au/quartz.Back to article page