Figure 4From: On the structure and oxygen transmission rate of biodegradable cellulose nanobarriersOTR as a function of density for films with a grammage of 20 g/m2. OTR was measured at 50% relative humidity. The measurements corresponding to the TEMPO-pretreated samples have been encircled.Back to article page