Skip to main content
Account

Table 1 Surface areas of prepared samples

From: Electrochemical performance of Ni x Co1-xMoO4 (0 ≤ x ≤ 1) nanowire anodes for lithium-ion batteries

 

Ni x Co1-xMoO4·n H2O

Ni x Co1-xMoO4

x value

Surface area (m 2 /g)

0

9.5

7.8

0.25

10.1

9.0

0.5

12.7

10.3

0.75

21.0

18.6

1

47.4

39.2

  1. Comparison of surface areas for as-prepared Ni x Co1-xMoO4·n H2O and Ni x Co1-xMoO4 nanowires dehydrated at 500°C for 2 h (by KS Park et al.).