Skip to main content
Account

Table 2 Samples obtained after further treatment on samples A and B (FGS)

From: Confident methods for the evaluation of the hydrogen content in nanoporous carbon microfibers

Sample

TA (K)

Atmosphere

P (bar)

tA (h)

F(A)

727

Ar

1

1

G(A)

927

Ar

0.2

2

H(G)

RT

H2

200

24

I(H)

RT

H2

0.00133

24

J(A)

RT

H2

200

24

K(B)

RT

H2

200

24

  1. Column 2 shows the annealing temperature, and the last column, the annealing time. RT, room temperature.