Figure 2From: Optimization of dye adsorption time and film thickness for efficient ZnO dye-sensitized solar cells with high at-rest stabilityXRD patterns of ZnO films. (A) Not sintered and (B) sintered at 400°C for 1 h. The asterisk denotes the FTO substrate.Back to article page