Table 3 The applied load versus penetration depth in loading stage

From: The evolution of machining-induced surface of single-crystal FCC copper via nanoindentation

 

Depth

0.5 nm

1.0 nm

1.5 nm

2.0 nm

Applied load to the indenter (nN)

Machining-induced surface

118.83

246.22

336.51

522.40

Pristine surface

167.74

268.15

487.05

530.47