Figure 3From: Femtosecond pulsed laser deposition of silicon thin filmsMicro-Raman spectroscopy of sample deposited at 200°C. Crystalline fraction found at approximately 520 cm −1 and the amorphous fraction at 480 cm −1, demonstrating a mixture of the two phases within the films.Back to article page