Table 1 PV parameters for Si solar cells after treatments
From: Improving Si solar cell performance using Mn:ZnSe quantum dot-doped PLMA thin film
Sample | ISC(mA) | UOC(V) | FF (%) | η(%) | Δ η/η0(%) | Δ η/η0(%) (calculated) |
---|---|---|---|---|---|---|
Bare cell | 66.50 | 0.59 | 73.65 | 11.12 | - | - |
CQD = 0 | 74.74 | 0.59 | 73.78 | 12.54 | 0.00 | 0.00 |
CQD = 1.6 mg/ml | 78.10 | 0.59 | 74.38 | 13.24 | 5.58 | 5.96 |
CQD = 3.0 mg/ml | 81.08 | 0.60 | 74.50 | 13.79 | 9.97 | - |