Figure 2From: Si nanopatterning by reactive ion etching through an on-chip self-assembled porous anodic alumina maskHigh magnification top view SEM image of sample 1. The PAA film thickness of sample 1 is 390 nm, and the average pore diameter is about 45 nm.Back to article page