Table 4 DRS studies: temperatures of the relaxation processes
From: Relaxation processes in hybrid organic-inorganic polymer nanosystems polymerized in situ
Compositions | Relaxation temperatures (ω = 1 Hz) | ||||
---|---|---|---|---|---|
Reactivity (R) | MDI (%) | PIC (%) | Tr0(°C) | Tr1(°C) | Tr2(°C) |
0.04 | 100 | 0 | −98 | −60 | - |
0.06 | 90 | 10 | −96 | −54 | - |
0.1 | 80 | 20 | −91 | −52 | 41 |
0.14 | 65 | 35 | −90 | −51 | 59 |
0.18 | 50 | 50 | −89 | −56 | 70 |
0.22 | 35 | 65 | −88 | −65 | 98 |
0.26 | 20 | 80 | −87 | −76 | 108 |