Table 2 List of BiNP samples grown at 0.12 W/cm 2 with different deposition temperatures

From: Size-controllable synthesis and bandgap modulation of single-layered RF-sputtered bismuth nanoparticles

Number

Substrate

T(°C)

P(W/cm2)

t(s)

Bi-301

ITO glass

160

0.12

60

Bi-302

ITO glass

200

0.12

60

Bi-303

c-Al2O3

160

0.12

60

Bi-304

c-Al2O3

200

0.12

60