Figure 1From: Electric charging/discharging characteristics of super capacitor, using de-alloying and anodic oxidized Ti-Ni-Si amorphous alloy ribbonsDSC trace and X-ray diffraction patterns. DSC trace of the studied amorphous Ti-Ni-Si alloy scanned at 0.67 K/s (a) and X-ray diffraction patterns of the studied alloy before and after de-alloying and then anodic oxidation (b).Back to article page