Table 1 Elemental relative concentration of Ag-covered L-CVD SnO 2 nanolayers at different steps of the procedure
From: XPS, TDS, and AFM studies of surface chemistry and morphology of Ag-covered L-CVD SnO2 nanolayers
Ag-doped L-CVD SnO2nanolayer procedures | Relative concentration | ||
---|---|---|---|
[O]/[Sn] | [C]/[Sn] | [Ag]/[Sn] | |
Freshly deposited | 1.30 ± 0.05 | 0.30 ± 0.05 | 0.50 ± 0.05 |
After exposure in dry air | 1.55 ± 0.05 | 3.50 ± 0.05 | 0.25 ± 0.05 |
After subsequent TDS | 1.30 ± 0.05 | 1.10 ± 0.05 | 0.15 ± 0.05 |