Figure 6From: Fabrication and sensing behavior of one-dimensional ZnO-Zn2GeO4 heterostructures Time-dependent current variation of the ZnO-ZGO heterostructures upon exposure to various acetone concentrations (50, 100, 250, 500, and 750 ppm) at 325°C. Back to article page