Figure 5

The NBE spectra of the as-grown and annealed ZnO NRs on AZO at 10 K. Inset: the integrated PL intensity of NBE as a function of reciprocal temperature for the annealed ZnO NRs, where the solid circles and the dashed line indicate experimental data and the fitting result to Equation 1, respectively.