Skip to main content

Table 1 Powders with different dopant concentrations

From: Microwave-Assisted Synthesis of Carbon-Based (N, Fe)-Codoped TiO2 for the Photocatalytic Degradation of Formaldehyde

Samples Anatase size (nm) Rutile size (nm) Ratio of A and R %
AC/TiO2 17.9 22.9 47/53
0.008 Fe-AC/TiO2 19.6 24.1 49/51
0.01 Fe-AC/TiO2 21.6 25.8 59/41
0.012 Fe-AC/TiO2 32.4 39.3 33/67
0.2 N-AC/TiO2 15.4 11.5 72/28
0.4 N-AC/TiO2 17.2 18.6 62/38
0.6 N-AC/TiO2 18.8 16.3 69/31