Table 1 Description of the studied samples
Sample | Description |
---|---|
P1 (powder) | Synthesis at 25 °С |
P2 (powder) | Synthesis at 80 °С |
T1 (coating) | Spraying of P2; distance to the Ti plate—150 mm |
T2 (coating) | Spraying of P2; distance to the Ti plate—200 mm |
T3 (coating) | Spraying of P1; distance to the Ti plate—150 mm |
T4 (coating) | Spraying of P1; distance to the Ti plate—200 mm |