Table 3 Summary of ANOVA results for the fitted responses

From: Evolution of Zinc Oxide Nanostructures Grown on Graphene by Ultrasonic Spray Pyrolysis and Its Statistical Growth Modelling

Source Nanorod density (ζ) Shape factor (φ) Nanorod size (r)
Prob > F Significance Prob > F Significance Prob > F Significance
Model <0.0001 Significance 0.019 Significance <0.0001 Significance
Q <0.0001 Significance 0.2458 Insignificance <0.0001 Significance
t <0.0001 Significance 0.1032 Insignificance <0.0001 Significance
M <0.0001 Significance 0.5334 Insignificance <0.0001 Significance
QM <0.0001 Significance 0.3644 Insignificance <0.0001 Significance
Qt NA NA 0.0149 Significance NA NA
Tt <0.0001 Significance NA NA NA NA
TM <0.0001 Significance 0.0229 Significance <0.0001 Significance
tM <0.0001 Significance NA NA <0.0001 Significance
Q 2 <0.0001 Significance 0.0559 Significance <0.0001 Significance
T 2 <0.0001 Significance 0.0092 Significance NA NA
t 2 <0.0001 Significance NA NA <0.0001 Significance
M 2 <0.0001 Significance 0.0252 Significance <0.0001 Significance
  1. NA not applicable