Table 1 Characteristics of PEDOT:PSS buffer layers prepared by regular spin coating and spin coating followed by substrate vibration post treatment (SVPT)
Sample no. | Vibration power (W) | Roughness (nm) | Thickness (nm) | Coverage (%) | Conductivity (S/cm) |
---|---|---|---|---|---|
1 | 5 | 21 | 45 | 96 | 565 |
2 | 0 | 70 | 140 | 68 | 82.5 |