Fig. 5From: Structure and Strength of Iron-Copper-Carbon Nanotube NanocompositesTensile strength σ В of the rolled Fe-Cu precursor 4:1 (1); Fe-Cu (4:1)-MCNT (0.5 vol.%) (2); Fe-Cu (4:1)-MCNT (1.0 vol.%) (3); Fe-Cu (4:1)-MCNT (1.5 vol.%) (4); and Fe-Cu (4:1)-MCNT (2.0 vol.%) (5) as a function of the treatment time of the respective component mixtures in the planetary millBack to article page