Table 1 Chemical composition of the starting materials and physical properties

From: Microstructure and Phase Composition of Cold Isostatically Pressed and Pressureless Sintered Silicon Nitride

Si3N4, wt%

Al2O3 wt%

Y2O3 wt%

Pressure (CIP), MPa

Powder bed

Temperature, °C

85

9

6

200

Si3N4

1650