Skip to main content

Table 1 Structural parameters of ZnAl LDHs

From: Organo/Zn-Al LDH Nanocomposites for Cationic Dye Removal from Aqueous Media

Sample a = 2d110, Å c = 3d003, Å Basal spacing d003, Å Interlayer distancea, Å Crystal size, Å
d003 d110
ZnAl LDH 3.074 22.8 7.60 2.8 172 198
ZnAl LDH reconstructed 3.073 22.7 7.55 2.8 174 122
ZnAl LDH/DS 3.068 78.6 26.20 21.4 152 162
  1. aInterlayer distance = d003—thickness of the brucite layer (4.8 Ǻ) [44]