Fig. 7From: The Effect of Mechanochemical Treatment of the Cellulose on Characteristics of Nanocellulose FilmsThermogravimetric analysis a heating curves, and b their first derivatives for the initial cellulose (1) initial cellulose after grinding to 93 °SR (2), cellulose after grinding and 43 % sulfuric acid hydrolysis (3), and cellulose after additional sonication (4)Back to article page