Table 3 PAL spectra parameterization of pelletized 0:5 nanocomposites (formed of pure ZnS) under channel width of 500 ns employing unconstrained x4- and x5-fitting procedures
PAL spectra fitting parameters | Ps trapping modes | |||||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
Lifetimes, ns | Intensities, % | R 3 | f 3 | R 4 | f 4 | R 5 | f 5 | |||||||
τ 1 | τ 2 | τ 3 | τ 4 | τ 5 | I 2 | I 3 | I 4 | I 5 | nm | % | nm | % | nm | % |
0.192 | 0.400 | 2.092 | 37.06 | – | 0.41 | 0.008 | 0.029 | – | 0.296 | 0.16 | 1.262 | 44.2 | – | – |
0.183 | 0.360 | 1.473 | 15.41 | 42.34 | 0.51 | 0.010 | 0.004 | 0.023 | 0.233 | 0.10 | 0.827 | 1.86 | 1.354 | 43.0 |