Fig. 6From: In Vitro Investigation of Bioactive Glass-Ceramic Composites Based on Biogenic Hydroxyapatite or Synthetic Calcium PhosphatesSaline pH change for different types of glass-ceramic composites samples for 120 min sample immersionBack to article page