Table 1 Oxidizing agent used in the reactive mixtures with H2SO4 and experimental conditions

From: Synthesis and Characterization of Highly Intercalated Graphite Bisulfate

Agent

HNO3

KNO 3

H2O2

KMnO4

Temperature reaction (°C)

40

30

40

30

Agent

K2Cr2O7

NaIO4

NaClO3

 

Temperature reaction (°C)

30

40

30

 