Skip to main content

Table 2 Thermogravimetric data of flexible PVC and PVC-matrix composites in air atmosphere

From: Titanate Nanotubes Decorated Graphene Oxide Nanocomposites: Preparation, Flame Retardancy, and Photodegradation

Sample T 5%/°C T 50%/°C T max1/°C T max2/°C
PVC 0 228 300 296 524
PVC 0.5 239 308 310 544
PVC 1.5 230 306 308 548
PVC 2.5 232 308 309 554
PVC 3.5 230 309 311 551