Fig. 9From: Enhanced performance of a novel anodic PdAu/VGCNF catalyst for electro-oxidation in a glycerol fuel cellPlot of the current density at the oxidation peak of the glycerol oxidation reaction (a) as a function of metal catalyst loading (wt.%) and NaOH concentration (M) at an electrolyte temperature of 80 °C and (b) as a function of electrolyte temperature (°C) and NaOH concentration (M) at 20 wt.% metal catalyst loadingBack to article page