Fig. 6From: Effect of Annealing on Microstructures and Hardening of Helium-Hydrogen-Implanted Sequentially Vanadium AlloysHardness in V-4Cr-4Ti alloys with different conditions. a Depth profiles of raw irradiation hardness. b Indentation depth of average nanoindentation hardness with error bar. c Plot of H2 vs 1/h for irradiated specimens. d Experimental ΔH measurements corrected for ISEBack to article page