Table 2 Test results of average particle/agglomerate size in suspensions

From: Graphene Oxide-Based Nanocomposites Decorated with Silver Nanoparticles as an Antibacterial Agent

Sample

Size by DLS, Z-average, diameter [nm] ± SD

Ag-NPs (as received)

80 ± 1

Ag-NPs (100 μg/mL, after US)

218 ± 93

GO (as received)

2030 ± 36

GO (200 μg/mL, after US)

263 ± 8

GO (200 μg/mL)-Ag (100 μg/mL)

251 ± 10

  1. DLS dynamic light scattering, Z-average harmonic intensity averaged particle diameter, SD standard deviation, US ultrasound method, Ag-NPs (as received) HydroSilver1000 (Amepox, Łódź, Poland) material was not processed Ag-NPs (100 μg/mL, after US) as above but was processed under US under similar conditions to the foils in the preceding sections, GO (as received) material not processed, GO (200 μg/mL, after US) as above but processed under US under similar conditions to the foils in the preceding sections, GO (200 μg/mL)-Ag (100 μg/mL) materials mixed together and processed under US under similar conditions to the foils in the preceding sections

Navigation