Table 2 Percentages of Si and O of different thermal oxidized Si sludge samples with different oxidation times. All data are before normalization

From: Transformation of sludge Si to nano-Si/SiOx structure by oxygen inward diffusion as precursor for high performance anodes in lithium ion batteries

Oxidation time (h)

5

7.5

10

Si weight percent (%)

71.05

65.48

60.12

O weight percent (%)

28.42

33.96

39.28

Si:O (mole ratio)

1:0.7

1:0.91

1:1.14