Table 2 Tensile strengths and elongation capacities of 30 wt% PNIPAM hydrogel composites with 0.02 wt% ZrO2 nano assembly
From: Nanoscale Effect of Zirconia Filler Surface on Mechanical Tensile Strength of Polymer Composites
Composite | Filler | StressMAX (kPa) | StrainMAX (%) |
---|---|---|---|
1 | – | 7.8 ± 0.2 | 716 ± 106 |
2b | Commercial ZrO2 | 7.7 ± 0.2 | 902 ± 28 |
3 | ZrO2 MARIMO | 9.2 ± 0.2 | 746 ± 37 |
4 | Sintered ZrO2 MARIMO | 6.6 ± 0.3 | 903 ± 19 |