Table 3 The PANI load rate of composites after several treatments
From: Synthesis of Polyaniline Coating on the Modified Fiber Ball and Application for Cr(VI) Removal
Sample-1 | Sample-2 | Sample-3 | |
---|---|---|---|
m0 (g) | 4.3030 | 3.5680 | 3.6771 |
m2 (g) | 4.5332 | 3.7476 | 3.8694 |
η2 (%) | 5.34 | 5.03 | 5.23 |